Tipless AFM Cantilevers
-
HQ:NSC35/tipless/No Al
Tipless AFM Probe with 3 Different Soft Tapping Mode AFM Cantilevers- 205/300/150 kHz 8.9/16/5.4 N/m
-
-
-
HQ:NSC36/tipless/No Al
Tipless AFM Probe with 3 Different Soft Tapping Mode AFM Cantilevers- 90/130/65 kHz 1.0/2.0/0.6 N/m
-
-
-
HQ:CSC37/tipless/No Al
Tipless AFM Probe with 3 Different Contact Mode AFM Cantilevers- 40/20/30 kHz 0.8/0.3/0.4 N/m
-
-
-
HQ:CSC38/tipless/No Al
Tipless AFM Probe with 3 Different Contact Mode AFM Cantilevers- 20/10/14 kHz 0.09/0.03/0.05 N/m
-
-
-
HQ:NSC35/tipless/Cr-Au
Tipless AFM Probe with 3 Different Gold Coated Soft Tapping Mode AFM Cantilevers- 205/300/150 kHz 8.9/16/5.4 N/m
-
-
-
-
HQ:NSC36/tipless/Cr-Au
Tipless AFM Probe with 3 Different Gold Coated Soft Tapping Mode AFM Cantilevers- 90/130/65 kHz 1.0/2.0/0.6 N/m
-
-
-
-
HQ:CSC37/tipless/Cr-Au
Tipless AFM Probe with 3 Different Gold Coated Contact Mode AFM Cantilevers- 40/20/30 kHz 0.8/0.3/0.4 N/m
-
-
-
-
HQ:CSC38/tipless/Cr-Au
Tipless AFM Probe with 3 Different Gold Coated Contact Mode AFM Cantilevers- 20/10/14 kHz 0.09/0.03/0.05 N/m
-
-
-
-
HQ:NSC35/tipless/Al BS
Tipless AFM Probe with 3 Different Soft Tapping Mode AFM Cantilevers- 205/300/150 kHz 8.9/16/5.4 N/m
-
-
-
HQ:NSC36/tipless/Al BS
Tipless AFM Probe with 3 Different Soft Tapping Mode AFM Cantilevers- 90/130/65 kHz 1.0/2.0/0.6 N/m
-
-
-
HQ:CSC37/tipless/Al BS
Tipless AFM Probe with 3 Different Contact Mode AFM Cantilevers- 40/20/30 kHz 0.8/0.3/0.4 N/m
-
-
-
HQ:CSC38/tipless/Al BS
Tipless AFM Probe with 3 Different Contact Mode AFM Cantilevers- 20/10/14 kHz 0.09/0.03/0.05 N/m
-
-
-
Videos
-
General view of the HQ:NSC35/Tipless and HQ:NSC36/Tipless AFM cantilevers
General view of the HQ:CSC37/Tipless and HQ:CSC38/Tipless AFM cantilevers
AFM Probe material
n-type silicon
AFM Probe bulk resistivity
0.01-0.025 Ohm*cm
The AFM probes in the Tipless series offer three different AFM cantilevers on one side of the chip without AFM tips. They can be used in various applications such as gluing microspheres or custom tip pyramids. HQ:NSC35 and HQ:NSC36 series AFM probes feature 3 different soft tapping mode AFM cantilevers, while HQ:CSC37 and HQ:CSC38 series AFM probes feature 3 different contact mode AFM cantilevers.
3 AFM Cantilevers Series
AFM Cantilever Resonance Frequency, kHz Force Constant, N/m min typical max min typical max 35 series Cantilever A 130 205 290 2.7 8.9 24 Cantilever B 185 300 430 4.8 16 44 Cantilever C 95 150 205 1.7 5.4 14 36 series Cantilever A 30 90 160 0.1 1.0 4.6 Cantilever B 45 130 240 0.2 2 9 Cantilever C 25 65 115 0.06 0.6 2.7 37 series Cantilever A 30 40 55 0.3 0.8 2 Cantilever B 15 20 30 0.1 0.3 0.6 Cantilever C 20 30 40 0.1 0.4 1 38 series Cantilever A 8 20 32 0.01 0.09 0.36 Cantilever B 5 10 17 0.003 0.03 0.13 Cantilever C 6 14 23 0.005 0.05 0.21 Application
Tipless AFM cantilevers are often used for custom applications such as for example attaching spheres or other objects for force spectroscopy measurements.